dc.description391-397en_US
dc.description.abstractBasic data on leaching of magnesite (MgCO3) with sulphuric acid are of interest from the point of view of the industrial process for obtaining pure MgSO4. The Taguchi method was used to determine the optimum conditions for the dissolution of magnesite in H2SO4 solutions. The experiments were performed within the ranges mentioned herein i.e. 20-65°C for reaction temperature, 0.5/100-10/100 g/mL for solid-to-liquid ratio, 0.2-5 M for acid concentration, 5-60 min for reaction time and 150-750 rpm for stirring speed. The optimum conditions for these factors were found to be 65°C, 5/100 g/mL, 2 M, 60 min and 300 rpm, respectively. Under these conditions, the dissolution mass fraction of MgCO3 in H2SO4 solutions were w = 96.32%.en_US
dc.language.isoen_USen_US
dc.publisherCSIRen_US
dc.relation.ispartofseriesC01B6/21en_US
dc.sourceIJCT Vol.13(4) [July 2006]en_US
dc.subjectOptimisationen_US
dc.subjectMagnesiteen_US
dc.subjectSulphuric aciden_US
dc.subjectTaguchi methoden_US
dc.titleDetermination of the optimum conditions for dissolution of magnesite with H2SO4 solutionsen_US
dc.typeArticleen_US
Appears in Collections:IJCT Vol.13(4) [July 2006]

Files in This Item:
File Description SizeFormat 
IJCT 13(4) 391-397.pdf226.56 kBAdobe PDFView/Open


Items in NOPR are protected by copyright, with all rights reserved, unless otherwise indicated.