dc.contributor.authorJahan, M Sarwar-
dc.contributor.authorChowdhury, D A Nasima-
dc.contributor.authorIslam, M Khalidul-
dc.contributor.authorHossain, S N-
dc.date.accessioned2009-07-23T08:39:11Z-
dc.date.available2009-07-23T08:39:11Z-
dc.date.issued2004-09-
dc.identifier.issn0975-1084 (Online); 0022-4456 (Print)-
dc.identifier.urihttp://hdl.handle.net/123456789/5498-
dc.description758-762en_US
dc.description.abstractSpent liquor of soda-monoethanolamine and soda-ethylenediamine processes were recirculated with white liquor in different proportions and its effect was studied on pulp properties and solid content in spent liquor. Pulp yield, kappa number, and solid contents in spent liquor were increased with increasing spent liquor recirculation. These increases were higher in soda-ethylenediamine process than that in soda-monoethanolamine process. There was not much significant change in strength properties up to 35 per cent of the spent liquor recirculation. The bleachability of the spent liquor recirculated pulp did not change much.en_US
dc.language.isoen_USen_US
dc.publisherCSIRen_US
dc.relation.ispartofseriesInt.Cl.7: C 02 F 1/00en_US
dc.sourceJSIR Vol.63(09) [September 2004]en_US
dc.subjectSpent liquoren_US
dc.subjectJuteen_US
dc.subjectSoda-amine pulpingen_US
dc.subjectPulpingen_US
dc.titleStudies on the spent liquor recirculation during soda-amine pulping of juteen_US
dc.typeArticleen_US
Appears in Collections:JSIR Vol.63(09) [September 2004]

Files in This Item:
File Description SizeFormat 
JSIR 63(9) 758-762.pdf61.46 kBAdobe PDFView/Open


Items in NOPR are protected by copyright, with all rights reserved, unless otherwise indicated.