dc.description1910-1913en_US
dc.description.abstractPoly(vinyl chloride) supported tetracycline sorbed zirconium(IV) selenomolybdate chelating inorganic exchange membrane has been employed for the determination of dysprosium(III) ion. The membrane electrode shows a Nernstain response for Dy(III) over a wide concentration range (l.0×10-1 M - 5×10-5 M) with a slope of 18.3 mV per decade of concentration. The detection limit is 3.8×10-5 M. The electrode is found to possess adequate stability and specific selectivity for Dy(III) over the other closely trivalent lanthanide metal ions with a response time of ~15 s. The sensor can also be used in partially non-aqueous medium, e.g., acetone/alcohol having 5- 10% (v/v) contents. Its working pH range is 2-9. It is successfully applied for the direct determination of Dy3+ in meta borate rock and as an indicator electrode in potentiometric titrations of dysprosium ion with 2-4 % experimental error.en_US
dc.language.isoen_USen_US
dc.publisherNISCAIR-CSIR, Indiaen_US
dc.rights CC Attribution-Noncommercial-No Derivative Works 2.5 Indiaen_US
dc.sourceIJC-A Vol.42A(08) [August 2003]en_US
dc.titlePoly(vinyl chloride) membrane containing zirconium(IV)selenomolybdate inorganic ion exchanger as dysprosium(III)ion selective electrodeen_US
dc.typeArticleen_US
Appears in Collections:IJC-A Vol.42A(08) [August 2003]

Files in This Item:
File Description SizeFormat 
IJCA 42A(8) 1910-1913.pdf925.02 kBAdobe PDFView/Open


Items in NOPR are protected by copyright, with all rights reserved, unless otherwise indicated.